Rolling contact fatigue (RCF) of the rail running surface is one of the major causes of rail damage and is currently of great importance in maintaining the reliability of railway tracks and affecting rail durability. As a result of high dynamic forces, small horizontal cracks form on the rail surface, which in the later stage of development pass vertically through the edge of the rail head, causing the formation of micro-fissures. In the event of a shortage of funds for diagnostics and failure to perform repairs within the specified time, these damages can be the cause of serious accidents. The article discusses the problems related to the formation and development of cracks, their identification, lists the factors influencing head check cracks, and explores possibilities for prevention and repair.In the last two decades, many countries have seen a revival of rail transport by providing faster, cheaper, more frequent, and more reliable connections for both passenger and freight transport. However, the increase in traffic intensity, higher speeds, and greater axle loads have a particular impact on the wear of the railway track, and thus on its maintenance and repair needs. (…)
The article contains 16,468 characters.
Source: Logistyka Magazine
Characteristics of head check rail cracks – PDF file for download