Case study of accelerated wear of a hoist rope

This paper presents the results of an investigation into a hoist rope. It was a steel rope withdrawn from service due to damage. The outer wires of the strands were undergoing elongation and cracking. The fractures should have been fatigue-related with deformation of the fracture zone, but instantaneous fractures without necking were observed, indicating material brittleness. The brittleness was observed only locally, therefore the probable cause was material inhomogeneity resulting from heat treatment.Steel ropes are frequently used for transport, especially vertical transport, of which hoist devices in mines are a specific type. Such devices are required to provide long-term, reliable operation under 24/7 usage. The second aspect is safety, especially when the device is used for transporting people.
The ropes used, depending on the design of the device and the depth of the shaft, have significant lengths, which affects their high price. At the same time, replacing ropes involves downtime of the device and brings measurable losses. Attempting to meet all criteria poses a challenge for the rope manufacturer. [1]2. MATERIAL AND RESEARCH METHODS
The subject of the study was a non-rotating rope Φ50 WS 6x + FE – Z/z (S/z)-n-I-g-1770 manufactured according to DIN 21254-9. The rope wires were covered with a zinc coating. The nominal strength should not be less than Rm = 1580 MPa. The nominal breaking force (…)

The article contains 16939 characters.

Source: Logistyka Magazine

Case study of accelerated wear of a hoist rope – PDF file for download